SA178a getemperte Wärmetauscher-Rohre ASTM A178 ERW
ContPerson : Richard SHEN
Telefonnummer : +86-13736164628
WhatsApp : +8613736164628
Min Bestellmenge : | 3 Tonnen | Preis : | negotiable |
---|---|---|---|
Verpackung Informationen : | Verpacken in der Holzkiste oder besonders angefertigt | Lieferzeit : | 20-45 TAGE |
Zahlungsbedingungen : | T/T, L/C, D/A, D/P, Western Union, MoneyGram | Versorgungsmaterial-Fähigkeit : | 50000 TONNEN PRO JAHR |
Herkunftsort: | Zhejiang, KN | Markenname: | TORICH |
---|---|---|---|
Zertifizierung: | ISO 9001,ISO14001,TS16949 | Modellnummer: | GRAD C ASTM A210 |
Detailinformationen |
|||
Produktname: | Kaltbezogene nahtlose Rifled Rohr-Wärmetauscher-Rohre | Schlüsselwort: | Rifled Rohr |
---|---|---|---|
Form: | Runde | Anwendung: | Für Kessel und Wärmetauscher |
Material: | GRAD C ASTM A210 | Oberfläche: | Besonders angefertigt |
Länge: | Max 12000mm | Rohr Od: | 8-400mm |
Flossen-Stärke: | 5-100mm | Marke: | TORICH |
Markieren: | rifled kaltbezogener nahtloser Schläuche,astm a210 kaltbezogener nahtloser Schläuche,astm a210 kaltbezogenes Stahlrohr |
Produkt-Beschreibung
Kaltbezogene nahtlose Rifled Rohr-Wärmetauscher-Rohre
Produkt-Name: Kaltbezogene nahtlose Rifled Rohr-Wärmetauscher-Rohre
Chemical&Mechanical-Parameter
Grad | C | Mangan | Si | Cr | MO | S | P |
20G | 0.17~0.23 | 0.35~0.65 | 0.17~0.37 | --- | --- | ≤0.020 | ≤0.025 |
20MnG | 0.17~0.23 | 0.70~1.00 | 0.17~0.37 | --- | --- | ≤0.020 | ≤0.025 |
25MnG | 0.22~0.29 | 0.70~1.00 | 0.17~0.37 | --- | --- | ≤0.020 | ≤0.025 |
12CrMoG | 0.08~0.15 | 0.40~0.70 | 0.17~0.37 | 0.40~0.70 | 0.40~0.55 | ≤0.020 | ≤0.025 |
15CrMoG | 0.12~0.18 | 0.40~0.70 | 0.17~0.37 | 0.80~1.10 | 0.40~0.55 | ≤0.020 | ≤0.025 |
SA-210A1 | ≤0.27 | ≤0.93 | ≥0.10 | --- | --- | ≤0.035 | ≤0.035 |
SA-210C | ≤0.35 | 0.29~1.06 | ≥0.10 | --- | --- | ≤0.035 | ≤0.035 |
SA-213T2 | 0.10~0.20 | 0.30~0.61 | 0.10~0.30 | 0.50~0.81 | 0.44~0.65 | ≤0.025 | ≤0.025 |
SA-213T12 | 0.05~0.15 | 0.30~0.61 | ≤0.50 | 0.80~1.25 | 0.44~0.65 | ≤0.025 | ≤0.025 |
Grad | T (MPa) | Y (MPa) | E (%) | Härte |
20G | 410~550 | 245 | ≥24 | --- |
20MnG | ≥415 | ≥240 | ≥22 | --- |
25MnG | ≥485 | ≥275 | ≥20 | --- |
12CrMoG | 410~560 | ≥205 | ≥21 | --- |
15CrMoG | 440~640 | ≥235 | ≥21 | --- |
SA-210C | ≥415 | ≥255 | ≥30 | ≤143HBW |
SA-210A1 | ≥485 | ≥275 | ≥30 | ≤179HBW |
SA-213T2 | ≥415 | ≥205 | ≥30 | ≤163HBW |
SA-213T12 | ≥415 | ≥220 | ≥30 | ≤163HBW |